bluing
英
美
n. 烤蓝; 蓝色漂白剂;上蓝剂; 蓝化;烧蓝;模温过高而引起的绿色氧化膜
COCA.46990
英英释义
noun
- a process that makes something blue (or bluish)
- used to whiten laundry or hair or give it a bluish tinge
双语例句
- The mechanism and treatment process as well as applying effect of bluing in alkaline media and blackening at room temperature for surface treatment of steel parts were contrasted, the optimal conditions and application using two surface treatment methods in the production were obtained.
本文作者旨在通过两种表面处理方法的形成机理、工艺流程以及运用效果的对比,得出两种方法在生产上的应用范围和适宜条件。 - Contrast between Bluing in Alkaline Media and Blackening at Room Temperature for Steel Parts
钢铁零件热碱发蓝与常温发黑的应用对比 - The causes of red exo-frost on bluing coating were analysed, which were higher content of main component in solution, more ferriferous oxide, smaller bluing tank volume, poor operation, repeated workpiece reworking, etc..
分析了发蓝膜层出现红色挂霜的原因:溶液主要成分含量过高、铁氧化物过多、发蓝槽容量小、工艺操作不当、工件多次返修等。 - Investigation on Bluing of Steel at Room Temperature In-Situ
常温原位发蓝研究 - BLUING/ BLUE UP: Process of using blue dye to coat a surface of a master, gauge, or piece of product to check a flat, circular, or tapered surface.
着色检查:使用蓝色染料涂在模具,量规或者产品表面以检查平面、圆面或者锥面的工序。 - Tapered bores for keyed hubs shall have a minimum of70% transfer of bluing ( surface contact) to the taper gage.
键槽轮毂的锥孔应至少有70%的着色(表面接触)转移到锥度计上? - Study of Basic Bluing Processing
关于碱性发兰工艺的分析 - Summary of Bluing Problem for Ammonium Bicarbonate Fertilizer
碳铵化肥发青问题解决小结 - Preventing red exo-frost on bluing coating
如何防止发蓝膜层的红色挂霜 - The production shows that the best bluing time in normal temperature is from 4 to 8 minutes and bluing film is bright and anti-corrosion capacity is at or higher than the specified state standard.
生产实践表明,常温发蓝的最佳发蓝时间为4~8分钟,发蓝膜光亮,耐蚀达到并超过国家规定标准。